Injection Molding 15 visualizaciones

Insufficient filling of PAR '2079851475616104452 (short shot)

Fenómeno del problema
The cavity is not completely filled and the product is short of material.
Análisis de la causa
The PAR melt viscosity is high, and the flowability is still limited at a processing temperature of around 300°C; the injection pressure and speed are insufficient.
Solución
Raise the melt temperature to 300-320°C; increase the injection pressure and speed; enlarge the gate and runner.
Conclusión clave
The high viscosity of PAR is the main cause of short shot.