Molds & Tooling 3 Aufrufe

Insufficient surface gloss of PAR products

Problembeschreibung
The surface gloss of the product is not as expected.
Ursachenanalyse
The mold temperature is low, the surface cools quickly and is not dense; the mold roughness is high.
Lösung
Raise the mold temperature to 130-160°C; mirror polish the mold; increase the injection speed.
Wichtigste Erkenntnis
High gloss of PAR requires high-temperature molds and mirror surfaces.
PARglossmold temperaturemirror surface