Extrusion & Post 3 Aufrufe

Annealing process of PAR products

Problembeschreibung
Insufficient annealing results in poor effects of eliminating internal stress and stabilizing dimensions.
Ursachenanalyse
The annealing temperature, time, or heating and cooling rate is improper.
Lösung
Anneal at 160-180°C for 2-4h with slow heating and cooling.
Wichtigste Erkenntnis
PAR annealing is a standard process for high-reliability applications.