Extrusion & Post 3 Aufrufe

PAR surface hardening coating

Problembeschreibung
PAR surface hardness is insufficient and needs coating protection.
Ursachenanalyse
PAR pencil hardness is around H, which cannot meet the harsh scratch resistance requirements.
Lösung
Apply UV or silane hard coating.
Wichtigste Erkenntnis
PAR surface strengthening is a high-end application requirement.
PARhardnesscoatingUV