Problembeschreibung
The surface activation treatment before chemical plating (copper and nickel plating) of PBT products is not in place, and the coating adhesion is poor.
Ursachenanalyse
The PBT surface is very inert and requires sufficient roughening treatment (chromic acid etching); the pre-treatment conditions (temperature, time, concentration) are improperly controlled.
Lösung
Optimize the roughening and etching process parameters (chromic acid-sulfuric acid system); ensure sufficient water washing; control the concentration of the activation solution.
Wichtigste Erkenntnis
PBT chemical plating pre-treatment is the key to bonding force.