Injection Molding 10 Aufrufe

Quality Fluctuation After Rapid Mold Change in PBT '2079851475616104452

Problembeschreibung
The quality of the first few shots or the first dozens of shots after mold change fluctuates greatly.
Ursachenanalyse
The new mold temperature is not stable; the hot runner temperature needs time to stabilize; the residual purging material affects the products of the initial shots.
Lösung
Fully preheat the mold after mold change; start production after the hot runner system stabilizes; discard the discharged material of the first few shots.
Wichtigste Erkenntnis
PBT quality stabilization after mold change requires a transition time.
PBTmold changequality fluctuationpreheatingdischarge