Problem Phenomenon
The quality of the first few shots or the first dozens of shots after mold change fluctuates greatly.
Cause Analysis
The new mold temperature is not stable; the hot runner temperature needs time to stabilize; the residual purging material affects the products of the initial shots.
Solution
Fully preheat the mold after mold change; start production after the hot runner system stabilizes; discard the discharged material of the first few shots.
Key Takeaway
PBT quality stabilization after mold change requires a transition time.