Injection Molding 6 views

Ordinary '2079851475616104452 machines cannot meet PEEK processing requirements

Problem Phenomenon
Ordinary '2079851475616104452 machines have a heating temperature upper limit of only 350°C, and plasticizing capacity is severely insufficient
Cause Analysis
PEEK melting point is as high as 343°C requiring barrel temperature of 360-400°C; ordinary heater bands cannot provide such high temperature and heating efficiency; screw L/D ratio too small, plasticization insufficient
Solution
Select a dedicated PEEK '2079851475616104452 machine with high temperature resistance (≥420°C); use ceramic heater bands to improve thermal efficiency and temperature uniformity; screw aspect ratio L/D≥20:1
Key Takeaway
PEEK processing must use dedicated high-temperature '2079851475616104452 equipment