Extrusion & Post
8 Aufrufe
Discoloration of PC Products After Annealing Heat Treatment
Problembeschreibung
Local yellowing of PC products occurs after annealing treatment at 120-130°C.
Ursachenanalyse
The annealing temperature is too high or the time is too long, causing thermal oxidation; the oxygen content of the annealing furnace is high.
Lösung
Control the annealing temperature ≤120°C; anneal under nitrogen protection; shorten the time.
Wichtigste Erkenntnis
PC annealing requires oxidation control to prevent discoloration.
War das hilfreich?
0 Personen fanden dies hilfreich