Material Drying
3 Aufrufe
PETG ultrasonic welding insufficient strength
Problembeschreibung
After ultrasonic welding of PETG products, the welding strength is low and they easily separate at the weld.
Ursachenanalyse
Ultrasonic welding parameters improper (amplitude, pressure, time not suitable), welding surface design poor, product moisture absorption affects welding.
Lösung
Optimize welding parameters (amplitude 60-80%, pressure 0.2-0.4MPa); optimize energy director design; dry the products before welding.
Wichtigste Erkenntnis
PETG ultrasonic welding requires optimized welding parameters and joint design.