Injection Molding
3 Aufrufe
Weld lines appear on PLA injection molded products
Problembeschreibung
The strength of the product at the weld line is low.
Ursachenanalyse
The temperature of the PLA melt is low when it converges and the fusion is poor, and the two melt fronts cannot be well combined.
Lösung
Raise the melt temperature to 190-200°C; raise the mold temperature; optimize the gate position to reduce weld lines.
Wichtigste Erkenntnis
PLA weld lines are related to the melt temperature and convergence conditions.