Injection Molding 3 Aufrufe

Formaldehyde odor and irritation in POM processing

Problembeschreibung
Strong formaldehyde pungent odor is produced during POM '2079851475616104452.
Ursachenanalyse
POM thermally decomposes at high temperature >210°C, releasing formaldehyde gas, especially when the barrel temperature is too high or residence is too long.
Lösung
Strictly control barrel temperature at 190-210°C not exceeding 230°C; shorten residence time; strong exhaust ventilation; use formaldehyde scavenger.
Wichtigste Erkenntnis
POM formaldehyde decomposition is the most prominent environmental and safety issue in processing.