Injection Molding 5 görüntüleme

Formaldehyde odor and irritation in POM processing

Sorun Belirtisi
Strong formaldehyde pungent odor is produced during POM '2079851475616104452.
Neden Analizi
POM thermally decomposes at high temperature >210°C, releasing formaldehyde gas, especially when the barrel temperature is too high or residence is too long.
Çözüm
Strictly control barrel temperature at 190-210°C not exceeding 230°C; shorten residence time; strong exhaust ventilation; use formaldehyde scavenger.
Temel Çıkarım
POM formaldehyde decomposition is the most prominent environmental and safety issue in processing.
POMformaldehydedecompositionodortemperature