POM melt fracture and rough surface
Problembeschreibung
Sharkskin-like roughness appears on the surface of POM products.
Ursachenanalyse
Excessively high extrusion or injection speed causes melt fracture; low die temperature; large shear rate.
Lösung
Reduce the injection/extrusion speed; raise the melt temperature and mold temperature; optimize the flow speed.
Wichtigste Erkenntnis
POM melt fracture is the consequence of over-shearing.