Molds & Tooling 3 Aufrufe

High haze of SBC transparent products

Problembeschreibung
The haze of SBC transparent products is on the high side, and transparency is not as expected
Ursachenanalyse
The SBC butadiene phase scatters light, causing haze Improper processing temperature intensifies phase separation and scattering Cooling rate is too fast, freezing a poor microstructure Excessive oil extension amount increases scattering Mold surface polishing is insufficient
Lösung
Select high-transparency SBC models (low butadiene content) Control processing temperature at 180-220°C to reduce phase separation Appropriately reduce the cooling rate Reduce the oil extension amount Polish the mold to mirror grade
Wichtigste Erkenntnis
SBC transparency needs to be addressed from model selection and phase separation