Molds & Tooling
3 Aufrufe
Sink marks and depressions on products
Problembeschreibung
Surface depressions and collapse appear at wall thickness changes or on the back of reinforcing ribs
Ursachenanalyse
Holding pressure or holding time is insufficient; premature gate solidification interrupts the shrinkage compensation channel; product wall thickness difference is too large, causing excessive local shrinkage
Lösung
Increase holding pressure and extend holding time by 30%; enlarge gate size to delay gate sealing; optimize product design for uniform wall thickness transition
Wichtigste Erkenntnis
The essence of sink marks is insufficient shrinkage compensation; in severe cases, it affects product mechanical strength
War das hilfreich?
0 Personen fanden dies hilfreich