Material Drying 3 Aufrufe

PAN precursor high breakage rate

Problembeschreibung
PAN fibers break frequently during wet or dry-wet spinning
Ursachenanalyse
The spinneret holes are clogged or scratched; the spinning solution contains gel or impurity particles; the coagulation bath conditions do not match, causing the skin layer to solidify prematurely
Lösung
Regularly clean and inspect the spinneret; filter the spinning solution through multiple stages (10μm→5μm→1μm); optimize the coagulation bath temperature and concentration
Wichtigste Erkenntnis
The quality of PAN precursor determines the grade of the final carbon fiber
breakagespinneretfiltrationcoagulation bathprecursor