Molding Process 3 Aufrufe

Sintered molded products cracking

Problembeschreibung
Pressureless sintered PEEK parts crack during sintering or after cooling
Ursachenanalyse
Uneven volume shrinkage during sintering heating (internal-external temperature difference); cooling rate too fast producing thermal stress; uneven density of the preformed green body
Lösung
Use slow and uniform heating rate (<3°C/min) and cooling rate; staged holding to homogenize the temperature field; increase pre-pressing pressure to improve green body density uniformity
Wichtigste Erkenntnis
The parameter control of the sintering process determines the success rate of PEEK pressureless molding
sinteringcrackingheating ratepre-pressingthermal stress