Molding Process
6 مشاهدة
Sintered molded products cracking
ظاهرة المشكلة
Pressureless sintered PEEK parts crack during sintering or after cooling
تحليل الأسباب
Uneven volume shrinkage during sintering heating (internal-external temperature difference); cooling rate too fast producing thermal stress; uneven density of the preformed green body
الحل
Use slow and uniform heating rate (<3°C/min) and cooling rate; staged holding to homogenize the temperature field; increase pre-pressing pressure to improve green body density uniformity
الخلاصة الأساسية
The parameter control of the sintering process determines the success rate of PEEK pressureless molding