Material Analysis 8 visualizaciones

ABAK flowability management

Fenómeno del problema
ABAK flowability is better than pure PA but is affected by the compatibilizer; as compatibilizer increases, flowability decreases.
Análisis de la causa
In the ABS-g-MAH compatibilized PA/ABS blend system, melt flowability decreases as compatibilizer dosage increases; the compatibilizer improves the interface but increases viscosity; flowability and mechanical properties need to be balanced; select high-flow grades.
Solución
①Optimize compatibilizer dosage without excess; ②select high-flow grades; ③appropriately increase the processing temperature; ④compensate with runner and gate design.; After adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
ABAK flowability and compatibility trade off against each other; optimized compatibilizer dosage is the key; grades and processes compensate for flowability.; After confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence
ABAK;flowability;compatibilizer;viscosity;grade;temperature