Material Drying 8 visualizaciones

ABAK BASF NM-19

Fenómeno del problema
ABAK BASF NM-19 high flow, high impact, UV-resistant grade; processing parameter reference.
Análisis de la causa
ABAK BASF NM-19; '2079851475616104452 temperature 240-280℃; drying 80-90℃×2-5h; mold temperature 62-82℃; high flow, high impact, UV resistant; automotive interior parts.
Solución
①Process according to supplier parameters; ②drying temperature and time; ③mold temperature control; ④performance verification; ⑤application matching.;after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Conclusión clave
The supplier parameters of ABAK commercial grades are the process benchmark; following them ensures quality; verification ensures application.;after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
ABAK;BASF;NM-19;high flow;UV resistant;parameters