Menú
Materiales Maquinaria
Perspectivas
Artículos Vídeos Problema y solución
About
Acerca de Chembull Socios de medios
Contáctenos
Idioma
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Volver a Problema y solución
Processing Machinery 8 visualizaciones

ABS cold slug mark

Fenómeno del problema
[Problem Phenomenon] ABS surface cold slug marks, front section disordered
Análisis de la causa
Nozzle temperature low or cold slug well insufficient; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
Solución
Match nozzle temperature to front section; enlarge cold slug well; raise injection speed; after adjustment, continuously sample to verify the effect, resume mass production only after confirming stability; change only one variable each time and record parameter changes to facilitate locating effective measures
Conclusión clave
For ABS cold slug marks check nozzle and cold slug well; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
cold slug mark nozzle cold slug well injection speed

¿Le ha resultado útil?

0 personas encontraron esto útil

ChemAI