Material Drying
8 visualizaciones
AEPDS drying management
Fenómeno del problema
AEPDS product silver streaks and bubbles, insufficient or excessive drying, improper hygroscopicity management.
Análisis de la causa
AEPDS hygroscopicity refers to ABS level; EPDM rubber phase influence; drying temperature and time need to match; excessive drying affects rubber phase; moisture content control.
Solución
①Dry at 80-90℃×3-4 hours; ②verify moisture content <0.1%; ③avoid excessive drying; ④sealed storage.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
AEPDS drying management refers to ABS but needs adjustment; verification ensures quality; prevent both excess and insufficiency.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence