Material Drying
8 visualizaciones
HDPE '2079851475616104457 parison streaks
Fenómeno del problema
Longitudinal light-colored streaks appear on the parison, and the product surface gloss is uneven.
Análisis de la causa
Excessive extrusion pressure/back pressure, high regrind ratio, raw material moisture or drying system abnormality, temperature control drift.
Solución
①Reduce extrusion pressure/back pressure; ②reduce the regrind ratio; ③test raw material moisture and the drying system; ④check the temperature controller.
Conclusión clave
Streaks are investigated along three lines: pressure, regrind, and moisture.
¿Le ha resultado útil?
0 personas encontraron esto útil