Injection Molding
15 visualizaciones
HDPE injection speed control
Fenómeno del problema
After high-speed injection the product is burnt near the gate, and at low speed flow marks and insufficient filling appear
Análisis de la causa
HDPE has good fluidity, but high-speed injection produces shear stress and molecular orientation, leading to uneven shrinkage; at low speed the front cools down and forms flow marks; medium-speed balance is the standard strategy
Solución
①Control the injection speed at medium speed; ②appropriately reduce the speed in the gate area to prevent shear; ③increase the melt temperature to compensate when flow marks appear; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
HDPE speed strategy is based on medium speed; the balance between shear and flow marks is achieved by a segmented speed curve; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence