Processing Machinery 8 visualizaciones

LDPE Ice Bag

Fenómeno del problema
Ice bags crack and leak after freezing
Análisis de la causa
Low-temperature freezing makes the film brittle, and the seal cracks first; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solución
Select low-temperature-resistant film; verify seal strength; freezing test; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate the effective measure
Conclusión clave
Frozen packaging uses low-temperature-resistant film; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
LDPEice baglow temperatureseal

¿Le ha resultado útil?