Material Drying
9 visualizaciones
PA6 Product Poor Surface Gloss
Fenómeno del problema
The surface was dull and not bright, failing to meet expectations.
Análisis de la causa
Low mold temperature and fast front cooling; or moisture silver streaks affecting gloss; insufficient surface replication; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Solución
①Appropriately increase mold temperature to improve the melt's replication and fit to the cavity surface;②strengthen drying and verify that the moisture content meets the standard with a moisture measurement method;③increase injection speed;④polish the cavity;⑤stabilize the material temperature curve to avoid quality drift caused by temperature fluctuation.
Conclusión clave
PA6 gloss = 'mold temperature + drying': mold temperature manages replication, drying manages surface state; moisture will drag down gloss, and drying is the prerequisite for gloss; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
¿Le ha resultado útil?
0 personas encontraron esto útil