Material Analysis 15 visualizaciones

PA6 Regrind Control

Fenómeno del problema
After blending regrind, product strength decreases, appearance black specks increase, and batch differences are large
Análisis de la causa
PA6 regrind decreases in molecular weight after experiencing thermal history, and performance cumulatively deteriorates after multiple cycles; regrind of unknown origin may also be mixed with other polymers and contaminants
Solución
①Control the regrind ratio within 20% and dry it separately; ②test melt index and impact strength by batch; ③restrict regrind use in load-bearing and appearance parts; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Conclusión clave
The value of PA6 regrind decreases with thermal history; ratio limitation, batch testing, and application grading are the three disciplines of regrind use; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence
PA6;regrind;thermal history;molecular weight;ratio control