Injection Molding 3 visualizaciones

PARA Incomplete Filling

Fenómeno del problema
Thin walls and ends of PARA products are underfilled; multiple links of shot size, pressure, speed, runner, temperature and venting may fail.
Análisis de la causa
Insufficient shot size; insufficient injection pressure and speed; too-small runner size; too-low material temperature with insufficient flowability; poor venting with air back pressure; 0.5mm thin-wall applications demand process limits.
Solución
①Increase shot size; ②Increase injection pressure and speed; ③Enlarge runner size; ④Increase material temperature; ⑤Add venting.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
PARA filling problems must be verified item by item along the systematic troubleshooting path; 0.5mm thin wall is the application boundary of the material's high flowability; when multiple factors superimpose, prioritize temperature and speed.
PARA; filling; short shot; thin wall; shot size; venting