Processing Machinery 7 visualizaciones

PCABS screw speed and shear

Fenómeno del problema
【Problem Phenomenon】PC/ABS screw high-speed shear generates heat, melt discolors and loses strength
Análisis de la causa
Medium-low screw speed is appropriate: high-speed shear heat degrades the PC phase; back pressure 5-15MPa to ensure uniform plasticization is enough, too high accumulates shear heat; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
Solución
Control screw speed at medium-low; back pressure 5-15MPa; for discoloration, first check speed and back pressure; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
PC/ABS screw medium-low speed with appropriate back pressure, shear heat is an invisible killer; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
screw speedback pressureshear heatdegradation