Material Drying 8 visualizaciones

PCABS Hydrolysis Resistance Evaluation

Fenómeno del problema
[Problem Phenomenon] The performance retention of PC/ABS parts in hot and humid environments is in doubt
Análisis de la causa
The PC phase in PC/ABS has hydrolysis sensitivity, and performance declines under long-term high temperature and high humidity; hot and humid working conditions require evaluation or selection of hydrolysis-resistant grades; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solución
Select hydrolysis-resistant grades for hot and humid parts; verify long-term hot and humid aging; dry processing to maintain molecular weight; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Conclusión clave
PC/ABS in hot and humid conditions needs evaluation, and hydrolysis-resistant grades are more stable; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
hydrolysis resistancehot and humidaginggrade

¿Le ha resultado útil?

0 personas encontraron esto útil

ChemAI