Menú
Materiales Maquinaria
Perspectivas
Artículos Vídeos Problema y solución
About
Acerca de Chembull Socios de medios
Contáctenos
Idioma
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Volver a Problema y solución
Material Drying 11 visualizaciones

PCABS Moisture Silver Streak Characteristics

Fenómeno del problema
[Problem Phenomenon] PC/ABS has silver-white hairline streaks randomly distributed over the entire surface, accompanied by water splash
Análisis de la causa
Characteristics of moisture-type silver streaks: randomly distributed over the entire surface, hairline-shaped, and splash-shaped in severe cases; PC hydrolysis also causes molecular weight decline and a sharp drop in impact strength; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solución
Immediately verify moisture content; if exceeding the standard, re-dry at 100-120°C for 3-4h; check hopper moisture regain and dryer dew point; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Conclusión clave
Moisture silver streaks are randomly distributed hairlines over the entire surface; drying re-testing is the first action; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
moisture silver streakshairline streaksdryinghydrolysis

¿Le ha resultado útil?

0 personas encontraron esto útil

ChemAI