PC Surface Hardness and Scratches
Fenómeno del problema
[Problem Phenomenon] PC product surface scratches
Análisis de la causa
PC surface hardness is medium and easily scratched; more obvious on high-gloss transparent parts; when troubleshooting on site, verify each item according to this mechanism one by one, and avoid blindly adjusting the machine based on experience alone; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solución
Protection during transfer; surface hardening coating; high-hardness grades; after adjustment, take samples continuously to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
Conclusión clave
PC fears scratches; protection plus hard coating; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!