PEI Thin-Walled Part Filling

Fenómeno del problema
PEI thin-walled connectors are difficult to fill; standard PEI cannot fill ultra-thin sections, forcing material changes or design modifications.
Análisis de la causa
PEI's high viscosity makes filling of ultra-thin walls (such as below 0.3mm) approach the physical limit of the material; standard grades have insufficient flowability; dedicated high-flow grades (such as GF15 modified high-flow grade) can improve but involve performance trade-offs.
Solución
①Evaluate dedicated high-flow grades; ②optimize gates and runners to the limit; ③utilize the upper limits of injection speed and pressure equipment; ④when truly infeasible, change the design or reselect the material.
Conclusión clave
PEI ultra-thin walls are a material limit challenge; high-flow grades are a feasible path; the trade-off between material performance and processability requires systematic evaluation.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PEI;thin wall;filling;high flow;grade;limit