Material Drying
7 visualizaciones
PET photovoltaic backsheet
Fenómeno del problema
PET film for photovoltaic backsheets yellows and chalks after ten years outdoors
Análisis de la causa
Long-term action of ultraviolet light and water vapor causes photo-oxidation and hydrolysis of PET; aging accelerates when the outer layer is unprotected; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solución
The backsheet uses fluorine-containing coating or composite structure to protect the PET substrate; verify by both damp heat and UV aging tests; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
Photovoltaic backsheets require composite protective structures; bare PET is not weather-resistant; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!