Processing Machinery
7 visualizaciones
POM Warpage Control
Fenómeno del problema
POM flat parts warp after ejection from the mold, with assembly flatness out of tolerance
Análisis de la causa
Uneven cooling of high-crystallinity material produces shrinkage differences, and warpage occurs after residual stress release; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry literature and should be confirmed first during troubleshooting
Solución
Balance cooling water circuits; raise mold temperature to 90℃; optimize holding pressure; anneal for setting if necessary; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
Warpage is controlled by cooling balance and sufficient crystallization; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!