Material Drying 7 visualizaciones

PPO Drying Equipment Selection

Fenómeno del problema
【Problem Phenomenon】Ordinary hot air oven drying of PPO has fluctuating effect, and defects rise again in the rainy season
Análisis de la causa
PPO moisture content requirement of 0.02% is a strict level, and ordinary hot air ovens are greatly affected by ambient humidity; dehumidifying dryers with stable dew point can ensure a consistent drying endpoint
Solución
Equip dehumidifying dryers and monitor dew point; hot air ovens are only used for low-requirement occasions with extended time; intensify moisture content sampling in the rainy season; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Conclusión clave
The 0.02% moisture content goal needs a dehumidifying dryer as backup; hot air ovens depend on the weather; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
dehumidifying dryerdew pointovenrainy season

¿Le ha resultado útil?

0 personas encontraron esto útil