Injection Molding 8 visualizaciones

PPO Flash and Clamping

Fenómeno del problema
[Problem Phenomenon] Flash at the parting line of PPO products; short shot reappears after pressure reduction
Análisis de la causa
PPO has high injection pressure requirements (100-140MPa), and flash occurs when clamping force is insufficient or the parting line is worn; the process window between high and low pressure is narrow; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solución
Calculate the clamping force margin against the projected area; repair the parting line fit; use a staged injection curve to balance filling and flash; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
PPO's high pressure requirement tests the clamping; when flash and short shot coexist, check the equipment first; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
flashclamping forceparting linehigh pressure