Fenómeno del problema
[Problem Phenomenon] Off-color and black specks after PP material/color change; incomplete cleaning
Análisis de la causa
Material and color changes require thorough cleaning; PP can use PE or dedicated purging compound; double for dark-to-light changes; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
Solución
Use PE or purging compound replacement for color changes; double for dark-to-light; synchronize the hot runner; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusión clave
Thorough cleaning for PP material changes; double for dark-to-light; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar future problems