Material Drying 9 visualizaciones

TPE Product Poor Surface Gloss

Fenómeno del problema
Product surface is foggy with insufficient gloss.
Análisis de la causa
Low polishing grade of cavity surface; low melt temperature and mold temperature, slow injection speed and insufficient '2079851475616104451 all affect gloss.; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
Solución
①Improve the cavity surface polishing grade; ②appropriately raise melt temperature and mold temperature; ③adopt higher injection speed; ④ensure the material is fully dried.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
Improving the polishing grade is the most direct method to improve gloss; process temperature, speed and drying cooperate for improvement.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
TPE;gloss;polishing;melt temperature;mold temperature;drying