TPE Bubbles
Fenómeno del problema
Bubbles appear inside or on the surface of products.
Análisis de la causa
Material moisture, poor venting or excessive injection pressure; when TPE oil content is high, volatile components also form bubbles.; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
Solución
①Strengthen raw '2079851475616104451; ②optimize mold venting; ③adopt multi-stage injection to reduce pressure; ④control the processing temperature.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusión clave
For TPE bubbles, check the three lines of moisture, venting and volatiles; drying and venting are the main countermeasures.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence