Processing Machinery 8 visualizaciones

TPE Barrel Zone Temperature

Fenómeno del problema
Uneven plasticization and cloud marks on products, or nozzle drooling and cold material spots on products
Análisis de la causa
TPE barrel zoning: rear zone 160-180℃, middle zone 170-200℃, front zone 180-220℃; nozzle temperature is independently controlled; improper zoning causes uneven plasticization or drooling
Solución
①Barrel rear zone 160-180℃, middle zone 170-200℃, front zone 180-220℃; ②Nozzle temperature slightly lower than the front zone; ③Cold slug well setting
Conclusión clave
TPE barrel zoning is the basis of uniform plasticization; the three-zone gradient plus independent nozzle temperature control, neither can be omitted; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
TPE; barrel temperature; zoning; nozzle; cold slug well