Insufficient EAA mixing
Fenómeno del problema
After blending EAA with fillers/additives, uneven dispersion and local agglomeration
Análisis de la causa
Insufficient length of the screw mixing section; insufficient number of kneading blocks; improper feeding method, additives not fully contacting EAA
Solución
1) Increase screw mixing section length to 3-4D; 2) Increase the number of kneading blocks; 3) Add additives through the side feeding port later to increase mixing time
Conclusión clave
Insufficient mixing is caused by improper screw design; increasing the mixing section is key