Material Analysis
15 visualizaciones
Unstable EEA shrinkage rate
Fenómeno del problema
EEA product shrinkage rate fluctuates ±0.8% exceeding the ±0.2% requirement
Análisis de la causa
Molecular weight difference between EEA batches causing shrinkage rate change; processing temperature fluctuation affecting crystallinity and thus the shrinkage rate
Solución
1) Strictly control raw material batch consistency; 2) Stabilize processing temperature ±2°C to ensure consistent crystallinity; 3) Reserve adjustment space for mold shrinkage compensation
Conclusión clave
Unstable shrinkage rate is caused by batch difference and temperature fluctuation; raw material and temperature control are key