Material Analysis 15 visualizaciones

EEA Hardness Too High

Fenómeno del problema
EEA product Shore hardness is 5-10 degrees higher than target, feels hard
Análisis de la causa
EEA crystallinity high, rigidity increased; too much filler added; cooling too fast, crystallization imperfect but rigidity frozen
Solución
1) Reduce cooling rate to make crystallization complete and reduce hardness feel; 2) Reduce filler addition; 3) Add 0.5wt% plasticizer to reduce hardness
Conclusión clave
High hardness is caused by crystallization and filler; adjusting cooling and filler are key
EEA high hardness crystallinity filler amount plasticizer