Material Analysis
15 visualizaciones
Strong EMA processing odor
Fenómeno del problema
Obvious pungent odor in EMA processing workshop
Análisis de la causa
EMA releases odorous volatiles at processing temperature (such as acetic acid, formaldehyde, etc.); additive decomposition releases odor
Solución
1) Control processing temperature within EMA recommended range to reduce decomposition; 2) Strengthen workshop ventilation and exhaust; 3) Add absorbent to neutralize odor
Conclusión clave
Strong odor is caused by EMA decomposition and volatilization; temperature control and ventilation are key