Injection Molding
7 visualizaciones
Periodic EMA surface ripples
Fenómeno del problema
Periodic ripples with 5-15mm spacing on EMA product surface
Análisis de la causa
Injection speed fluctuates periodically; hydraulic system unstable; screw speed unstable
Solución
1) Overhaul injection system to stabilize pressure and speed; 2) Servo motor drive replacing hydraulic drive; 3) PID control to stabilize injection parameters
Conclusión clave
Ripples are caused by unstable injection; equipment overhaul and PID control are key
¿Le ha resultado útil?
0 personas encontraron esto útil