Injection Molding 2 visualizaciones

Insufficient flow length ratio in EVA '2079851475616104452

Fenómeno del problema
EVA '2079851475616104452 flow length ratio only 80-100, below 150; thin wall products cannot be filled
Análisis de la causa
EVA melt viscosity high with short flow distance; injection temperature too low; injection pressure insufficient; mold runner resistance large
Solución
1) Increase injection temperature to 140-200°C; 2) Increase injection pressure to 80-100MPa; 3) Enlarge runner and gate size to reduce resistance; 4) Add 0.3-0.5wt% flow aid to reduce viscosity
Conclusión clave
Insufficient flow length ratio is caused by EVA high viscosity; high temperature, high pressure and large gate are key
EVA injection flow length ratio melt viscosity injection temperature flow aid