Material Analysis
15 visualizaciones
Insufficient EVOH Toughness, Brittle Fracture
Fenómeno del problema
EVOH product elongation at break <50%, brittle fracture without yielding
Análisis de la causa
EVOH molecular weight too low, toughness foundation insufficient; crosslinking excessive losing toughness; crystallization coarse increasing brittleness
Solución
1) Select high molecular weight EVOH to improve toughness; 2) Control crosslinking degree to avoid excess; 3) Nucleating agent to refine crystallization and improve toughness
Conclusión clave
Insufficient toughness is caused by low molecular weight and coarse crystallization; selecting high MW is key
¿Le ha resultado útil?
0 personas encontraron esto útil