Injection Molding
2 visualizaciones
Ejector whitening of PVA injection molded products
Fenómeno del problema
PVA injection molded product shows white marks at ejector pin positions, ejector whitening affecting appearance
Análisis de la causa
Excessive ejector pin force causes local compression deformation and whitening; insufficient cooling time, product ejected before fully solidified; ejector pin area too small causing stress concentration
Solución
1) Extend cooling time so the product is fully solidified before ejection; 2) Increase ejector pin area, use ejector plate instead of small ejector pins; 3) Reduce ejection speed to reduce impact force; 4) Increase draft angle to reduce ejection force
Conclusión clave
Ejector whitening is caused by excessive ejection force and insufficient cooling; increasing ejector pin area and extending cooling time are the key
¿Le ha resultado útil?
0 personas encontraron esto útil